Influence of Temperature on the Performance of LiNi1/3Co1/3Mn1/3O2 Prepared by High-Temperature Ball-Milling Method
Figure 4
SEM images of products prepared at various temperatures of (a) 700°C, (b) 750°C, (c) 800°C, and (d) 850°C.