Research Article

Influence of Temperature on the Performance of LiNi1/3Co1/3Mn1/3O2 Prepared by High-Temperature Ball-Milling Method

Table 1

Lattice parameter of LiNi1/3Co1/3Mn1/3O2 powders prepared at various temperatures.

Na-axis (Å)c-axis (Å)c/a ratio

700°C2.864214.18954.954
750°C2.865314.23844.969
800°C2.866114.23634.967
850°C2.866714.22954.964