The Influence of a Thermal Treatment on the Decay Resistance of Wood via FTIR Analysis
Table 3
Contents of the nutrients in untreated and heat-treated specimens.
| Initial MC/heating temperatures | Nutrient | Untreated | 5%/180°C | 15%/180°C | 30%/180°C | 5%/200°C | 15%/200°C | 30%/200°C | 5%/220°C | 15%/220°C | 30%/220°C |
| Lignin | 0.2071 | 0.2042 | 0.2012 | 0.2005 | 0.201 | 0.1995 | 0.1958 | 0.196 | 0.195 | 0.1951 | Cellulose | 0.5059 | 0.4999 | 0.4994 | 0.4819 | 0.479 | 0.4806 | 0.4661 | 0.437 | 0.413 | 0.4164 | Holocellulose | 0.7840 | 0.5487 | 0.547 | 0.5274 | 0.517 | 0.5154 | 0.4993 | 0.471 | 0.44 | 0.4424 | Hemicellulose | 0.2782 | 0.0488 | 0.0477 | 0.0455 | 0.038 | 0.0349 | 0.0331 | 0.033 | 0.027 | 0.026 |
|
|