Research Article

Protective Ceramic Coatings for Solid Oxide Fuel Cell (SOFC) Balance-of-Plant Components

Figure 13

YSZ-coated 430 stainless steel. (a) Edge; (b) center of the sample after four (4) deposition cycles using dip coating. (c) Edge; (d) center of the sample after five (5) deposition cycles using dip coating. (e) Edge; (f) center of the sample after two (2) deposition cycles using dip coating. (g) Edge; (h) center of the sample after three (3) deposition cycles using dip coating. (i) Edge; (j) center of the sample after four (4) deposition cycles using dip coating.