Research Article
(Co,Mn)3O4 Spinel Coating for Protecting Metallic Interconnects Thermally Converted from an Electro-Codeposited Co-Mn3O4 Composite Coating
Figure 6
Cross-sectional morphology and EDS linear scan of the plated substrates after thermal conversion for different times: (a) the Co coating for 10 min; (b) the Co coating for 4 h; (c) the Co-Mn3O4 coating for 10 min; and (d) the Co-Mn3O4 coating for 4 h.