Mix proportion of rubber concrete in experiment (unit: kg/m3).
| Number | Rubber | Cement | Sand | Water | Water reducer | Agglomerant |
| O | 0 | 380 | 1900 | 133 | 5.7 | 0 | A | 120.9 | 380 | 1760.9 | 133 | 5.7 | 18.1 | B | 241.9 | 380 | 1621.9 | 133 | 5.7 | 36.3 | C | 362.8 | 380 | 1482.8 | 133 | 5.7 | 54.4 | D | 483.7 | 380 | 1343.7 | 133 | 5.7 | 72.6 | E | 604.7 | 380 | 1204.6 | 133 | 5.7 | 90.7 | F | 725.6 | 380 | 1065.6 | 133 | 5.7 | 108.8 | H | 967.5 | 380 | 787.4 | 133 | 5.7 | 145.1 |
|
|