Synthesis of Ti2SnC under Optimized Experimental Parameters of Pressureless Spark Plasma Sintering Assisted by Al Addition
Figure 9
SEM and EDS micrographs of Ti2SnC with ratio Ti : Sn : Al : C = 2 : 1 : 0.2 : 1 at (a and b) 800°C, (c and d) 1000°C, and (e and f) 1200°C.