Research Article

Investigation of Bioactive Glass-Ceramic 60SiO2-30CaO-10P2O5 Prepared by Hydrothermal Method

Figure 8

Evaluations of pH and Ca, Si, and P concentrations in the SBF solution after 0, 7, 14, and 20 days.
(a)
(b)
(c)
(d)