Research Article
Hot Deformation Behavior and Microstructural Evolution of Twin-Roll-Casting Mg Alloy during High-Temperature Compression
Figure 2
True stress-true strain curves of the TRC-AZ31 alloy during hot compression at 450°C: (a) 5% strain; (b) 15% strain; (c) 25% strain; (d) 35% strain.
(a) |
(b) |
(c) |
(d) |