Research Article

Effect of Heat Treatment and Titanium Addition on the Microstructure and Mechanical Properties of Cast Fe31Mn28 Ni15Al24.5Tix High-Entropy Alloys

Figure 3

Scanning electron micrographs of the as-cast samples (a) 0.0 and (b) 3.0 wt.% Ti at 30 mm and (c) 0.0 wt.% Ti sample at 5 mm.
(a)
(b)
(c)