Research Article
Effects of Continuous Laydown and Compaction on Interlayer Shear Bonding of Asphalt Layers
Table 9
Summary of interlayer adhesion test results.
| Specimen type | 13/16 | 16/20 | AC13 | AC16 | AC20 | Bonding layer | Not bonding layer | C. pave | Disc. pave | C. pave | Disc. pave |
| τ (MPa) | Room T. | 0.252 | 0.121 | 0.222 | 0.089 | 0.255 | 0.293 | 0.314 | Standard deviation | 0.028 | 0.014 | 0.026 | 0.011 | 0.021 | 0.016 | 0.024 | Low T. | 1.828 | 1.230 | 1.897 | 0.772 | 1.690 | 1.813 | 1.829 | Standard deviation | 0.13 | 0.09 | 0.148 | 0.062 | 0.11 | 0.16 | 0.15 | Freeze-thaw | 0.116 | 0.016 | 0.048 | 0.014 | 0.083 | 0.108 | 0.098 | Standard deviation | 0.014 | 0.003 | 0.009 | 0.0028 | 0.019 | 0.01 | 0.011 |
|
|