Research Article
Factors Influencing the Rheological Properties of MRSP Based on the Orthogonal Experimental Design and the Impact Energy Test
Figure 1
(a) The MRSP sample at a room temperature, (b) SEM image of the internal microstructure, and (c) FTIR spectrum in the range of 4000–500 cm−1.
(a) |
(b) |
(c) |