Factors Influencing the Rheological Properties of MRSP Based on the Orthogonal Experimental Design and the Impact Energy Test
Figure 5
(a) The RSE of the continuously changing angular frequency from 0.1 to 100 rad/s and (b) the RME of the continuously changing magnetic flux density from 0 to 1000 mT with different PDMS viscosities.