Research Article
Mechanical Recovery of Cracked Fiber-Reinforced Mortar Incorporating Crystalline Admixture, Expansive Agent, and Geomaterial
Figure 6
Load versus CMOD for specimens of all mix types, healed for durations of 28 or 56 days: (a) OPC, 28 days; (b) OPC, 56 days; (c) SH1, 28 days; (d) SH1, 56 days; (e) SH2, 28 days; (f) SH2, 56 days.
| (a) | 
| (b) | 
| (c) | 
| (d) | 
| (e) | 
| (f) |