Research Article
Study on the Preparation and Fracture Behavior of Red Mud-Yellow Phosphorus Slag-Based Concrete
Figure 12
The field displacement of the first crack area and surface topographies on the RM-YPS-CC surface at the age of 28 days under (a) 5 MPa; (b) 10 MPa; (c) 15 MPa; (d) 20 MPa; (e) 25 MPa; and (f) 30 MPa.
| (a) |
| (b) |
| (c) |
| (d) |
| (e) |
| (f) |