Research Article
The Dosage of Superplasticizer in Cemented Coal Waste Backfill Material Based on Response Surface Methodology
Table 3
Design of tests based on CCD and test results.
| Run | Design of tests | Results of tests | A | B | C | SP (% of binder) | Slump flow (mm) | VSI |
| 1 | 1.000 | 1.000 | 1.000 | 0.702 | 440 | 0 | 2 | −1.000 | 1.000 | 1.000 | 0.526 | 420 | 0 | 3 | 0.000 | 0.000 | 0.000 | 0.521 | 450 | 0 | 4 | 0.000 | 1.682 | 0.000 | 0.667 | 430 | 0 | 5 | −1.682 | 0.000 | 0.000 | 0.281 | 430 | 0 | 6 | 1.000 | −1.000 | −1.000 | 0.075 | 470 | 1 | 7 | 0.000 | 0.000 | 1.682 | 1.253 | 420 | 0 | 8 | 0.000 | 0.000 | −1.682 | 0.000 | 540 | 2 | 9 | 0.000 | 0.000 | 0.000 | 0.521 | 460 | 0 | 10 | 0.000 | −1.682 | 0.000 | 0.596 | 460 | 0 | 11 | 0.000 | 0.000 | 0.000 | 0.521 | 445 | 0 | 12 | 0.000 | 0.000 | 0.000 | 0.521 | 450 | 0 | 13 | −1.000 | −1.000 | 1.000 | 1.003 | 465 | 0 | 14 | 1.000 | −1.000 | 1.000 | 1.053 | 460 | 0 | 15 | −1.000 | 1.000 | −1.000 | 0.351 | 475 | 1 | 16 | 1.000 | 1.000 | −1.000 | 0.251 | 500 | 1 | 17 | −1.000 | −1.000 | −1.000 | 0.000 | 440 | 1 | 18 | 1.682 | 0.000 | 0.000 | 0.602 | 450 | 0 | 19 | 0.000 | 0.000 | 0.000 | 0.521 | 450 | 0 | 20 | 0.000 | 0.000 | 0.000 | 0.521 | 445 | 0 |
|
|