Research Article
The Dosage of Superplasticizer in Cemented Coal Waste Backfill Material Based on Response Surface Methodology
Table 4
ANOVA of response surface quadratic model for SP.
| | Sum of squares | df | Mean square | F value | value |
| Model | 0.4303 | 6 | 0.0717 | 63.68 | <0.0001 | A | 0.0091 | 1 | 0.0091 | 8.12 | 0.0137 | B | 0.0023 | 1 | 0.0023 | 2.07 | 0.1741 | C | 0.3467 | 1 | 0.3467 | 307.88 | <0.0001 | BC | 0.0522 | 1 | 0.0522 | 46.39 | <0.0001 | A2 | 0.0081 | 1 | 0.0081 | 7.21 | 0.0187 | C2 | 0.0135 | 1 | 0.0135 | 11.97 | 0.0042 | Residual | 0.0146 | 13 | 0.0011 | | | Lack of fit | 0.0146 | 8 | 0.0018 | | <0.0001 | Pure error | | 5 | | | | Cor total | 0.4449 | 19 | 7.916 ∗ 11 | | |
|
|
Standard deviation: 0.0336; R2: 0.9671; adjusted (R2): 0.9519; adequate precision: 27.8528.
|