Rutting and Fatigue Properties of Cellulose Fiber-Added Stone Mastic Asphalt Concrete Mixtures

Table 2

FN test results.

MixturesFN value (seconds)Accumulated strain@FN (microstrains)
CorrectedAMPTAMPT

25 mm1000011044
19 mm1000010194
12.5 mm1712237535819