Advances in Materials Science and Engineering / 2019 / Article / Tab 2 / Research Article
Optimization of Low-Carbon Footprint Quaternary and Quinary (37% Fly Ash) Cementitious Nanocomposites with Polycarboxylate or Aqueous Nanosilica Particles Table 2 Mix proportions (%) by total mass of solids.
PC (%) LS (%) FA (%) μ S (%)nS (% solids) w/b Mix PC43LS20FA43 (0% nS) 43 20 37 0.0 0.0 0.3 Quaternary mixes PC43LS19.9FA37 + 0.1% nS 43 19.9 37 0.0 0.1 0.3 PC43LS19.8FA37 + 0.2% nS 43 19.8 37 0.0 0.2 0.3 PC43LS19.5FA37 + 0.5% nS 43 19.5 37 0.0 0.5 0.3 PC43LS19FA37 + 1.0% nS 43 19 37 0.0 1.0 0.3 Quinary mixes PC43LS17FA37 + 2.5% μ S + 0.5% nS 43 17 37 2.5 0.5 0.3 PC43LS17FA37 + 2.0% μ S + 1.0% nS 43 14 37 2.0 1.0 0.3 PC43LS14FA37 + 5.5% μ S + 0.5% nS 43 14 37 5.5 0.5 0.3 PC43LS14FA37 + 5.0% μ S + 1.0% nS 43 17 37 5.0 1.0 0.3