Research Article
Elements-Added Diamond-Like Carbon Film for Biomedical Applications
Table 5
Surface contact angle, corrosion potential (Ecorr), and corrosion current density (icorr) of pure DLC, Si-DLC, and Si-N-DLC films.
| Film type | Gas flow rate ratio | Contact angle (°) | Corrosion potential (Ecorr (V)) | Corrosion current density (icorr (A/cm2)) |
| Uncoated AISI316L | — | 93.47 | −0.125 | 2.49E − 6 |
| Pure DLC | — | 79.33 | −0.010 | 0.949E − 6 |
| Si-DLC | 1 : 2 | 88.93 | 0.198 | 0.887E − 6 | 1 : 4 | 92.20 | 0.199 | 0.909E − 6 | 1 : 6 | 92.47 | 0.398 | 0.280E − 6 |
| Si-N-DLC | 14 : 1 : 2 | 77.87 | −0.001 | 0.931E − 6 | 14 : 1 : 4 | 76.23 | 0.004 | 0.648E − 6 | 14 : 1 : 6 | 77.53 | 0.198 | 0.570E − 6 |
|
|