Research Article
Surface Laser Processing of Additive Manufactured 1.2709 Steel Parts: Preliminary Study
Table 3
Calculated energy density (J/cm2).
| Scanning speed V, mm/s | Laser power P, W | Level of energy input | 2 | 2.5 | 3 |
| 1 | 13600 | 17000 | 20400 | E3 | 2,5 | 5440 | 6800 | 8160 | E2 | 5 | 2720 | 3400 | 4080 | E1 |
|
|