Research Article
Surface Laser Processing of Additive Manufactured 1.2709 Steel Parts: Preliminary Study
Table 4
Elemental composition of initial powder and surface of samples (by EDS, in weight%).
| Sample | Element | Fe | Ni | Co | Mo | Ti | O |
| Powder for SLS | Balance | 20 | 6.9 | 4.5 | 0.7 | 2.0 | As-manufactured SLS sample | 23 | 8.2 | 4.1 | 0.7 | 5.1 | C4 (2.5 W/1 mm/s) | 14.9 | 10.6 | 3.1 | 1.26 | 26.0 | C5 (2.5 W/2.5 mm/s) | 11.8 | 6.1 | 4.0 | 0.8 | 24.0 | C6 (2.5 W/5 mm/s) | 10.4 | 7.6 | 2.3 | 0.6 | 22.1 |
|
|