Research Article
Fretting Wear Behavior and Damage Mechanisms of Inconel X-750 Alloy in Dry Contacts
Figure 10
SEM micrographs of Inconel X-750 wear scars during PSR: (a) after 10 minutes, (b) after 30 minutes, and (c) after 90 minutes of fretting. Displacement amplitude is 40 µm. Double arrows represent fretting direction.
(a) |
(b) |
(c) |