Research Article

Preparation of a Cenosphere Curing Agent and Its Application to Foam Concrete

Table 3

The main chemical composition of cenospheres before and after chemical corrosion (wt.%).

CompositionSiO2Al2O3CaOFe2O3TiO2MgONa2OK2OP2O5

Original cenospheres58.3531.430.432.261.180.530.551.410.05
Perforated cenospheres58.8134.500.322.121.160.500.531.320.05