Research Article

Fatigue Life Behavior of Laser Shock Peened Duplex Stainless Steel with Different Samples Geometry

Figure 15

Fracture surfaces of the 4 mm thick specimen: (a, d) crack initiation, (b, e) fatigue striation, and (c, f) final rupture. Figure 15 is reproduced from Granados-Alejo et al. [19].