| Reinforcement grade | Application | Diameter (mm) | Yield strength (MPa) | Ultimate strength (MPa) |
| 600 | Longitudinal bars | 22 | 612.5 | 796.4 | 600 | Longitudinal bars | 20 | 633.3 | 824.9 | 600 | Longitudinal bars | 14 | 651.0 | 861.7 | 400 | Longitudinal bars | 22 | 455.8 | 625.9 | 400 | Longitudinal bars | 20 | 441.9 | 588.6 | 400 | Longitudinal bars | 14 | 423.4 | 632.4 | 300 | Transverse stirrups | 10 | 360.6 | 522.2 | 300 | Transverse stirrups | 6 | 353.6 | 398.3 |
|
|