Directional Solidification of Sn-Cu6Sn5 In Situ Composites
Figure 2
Longitudinal view of Sn-7 wt.% Cu samples directionally grown at increasing values of pulling velocity: (a) 1.0 µm/s; (b) 2.0 µm/s; (c) 5.0 µm/s (GL = 2.5 K/mm).
(a) |
(b) |
(c) |