Research Article

Microstructural and Mechanical Analysis of Sintered Powdered Aluminium Composites

Table 2

Samples of 5% SiC reinforcement.

Raw metal powdersAtomic numberDensity (ρ) in gm/cm3Weight percentages (%) in mixture (x)Rule of mixture (ρ × x) in gm/cm3

Aluminium (Al)132.7091.52.4705
Copper (Cu)298.962.50.224
Magnesium (Mg)141.7380.50.00869
Silicon (Si)122.3290.50.011648
Silicon carbide (SiC)3.2150.1605
Total1002.875338