Research Article
Study on the Mechanical Properties of Metal Rubber Inner Core of O-Type Seal with Large Ring-to-Diameter Ratio
Table 2
Change of loss factor and energy dissipation with porosity after heat treatment.
| Porosity (%) | Loss factor (room temperature, heat treatment) η | Energy dissipation (room temperature, heat treatment) |
| 51.5 | 0.26442, 0.21857 | 0.05371, 0.03574 | 57.6 | 0.27501, 0.19054 | 0.06469, 0.03234 | 63.7 | 0.30210, 0.18699 | 0.06688, 0.01979 | 69.7 | 0.32120, 0.14297 | 0.06893, 0.01519 |
|
|