Research Article

The Effect of α-Al(MnCr)Si Dispersoids on Activation Energy and Workability of Al-Mg-Si-Cu Alloys during Hot Deformation

Figure 13

SEM micrographs of WQ1 compressed at 300°C with 0.1 s−1 to strain of 1: (a) particle cracking and debonding; (b) micro cracks.
(a)
(b)