The Effect of α-Al(MnCr)Si Dispersoids on Activation Energy and Workability of Al-Mg-Si-Cu Alloys during Hot Deformation

Figure 8

Processing maps of 6061 (a) and WQ1 (b) developed at the true strain of 1.2.