The Effect of α-Al(MnCr)Si Dispersoids on Activation Energy and Workability of Al-Mg-Si-Cu Alloys during Hot Deformation
Figure 9
EBSD maps (a, b), misorientation angle distribution (c, d), and substructures (e, f) of 6061 (a, c, e) and WQ1 (b, d, f) alloys compressed at 550°C and 10 s−1 to strain of 1.2. The inset in (a) is inversed pole figure coloring.
(a) |
(b) |
(c) |
(d) |
(e) |
(f) |