Research Article
The Effect of α-Al(MnCr)Si Dispersoids on Activation Energy and Workability of Al-Mg-Si-Cu Alloys during Hot Deformation
Table 3
Safe processing domains of 6061 and WQ1.
| Alloys | Low strain rate domains (I & II) | High strain rate domains (III) |
| 6061 | 485–550°C, 0.01–0.08 s−1 | 530–550°C, 6–10 s−1 | 440–480°C, 0.05–0.6 s−1 | | WQ1 | 485–550°C, 0.01–0.1 s−1 | |
|
|