Research Article

Shrinkage and Strength Properties of Coal Gangue Ceramsite Lightweight Aggregate Concrete

Figure 15

Shrinkage of the concrete with (a) drying and (b) CGC prewetting (24 h) at 56 d.
(a)
(b)