Research Article
Effects of Graphene Oxide Dispersion on Salt-Freezing Resistance of Concrete
Figure 3
Macroscopic failure characteristics of GO concrete under different salt-freezing cycles. (a) 50 salt-freezing cycles. (b) 100 salt-freezing cycles. (c) 150 salt-freezing cycles. (d) 200 salt-freezing cycles.
(a) |
(b) |
(c) |
(d) |