Research Article

Evolution of Dynamic Recrystallization in 5CrNiMoV Steel during Hot Forming

Figure 11

Optical microstructure of 5CrNiMoV steel deformed at the strain rate of 1 s−1: (a) T = 830°C, (b) T = 930°C, (c) T = 1030°C, (d) T = 1130°C, and (e) T = 1230°C.