Research Article
Protective Cerium-Based Layered Double Hydroxides Thin Films Developed on Anodized AA6082
Figure 10
Electrical equivalent circuits employed to fit the EIS experimental dataset: (a) at the early stage of immersion (1–120 h) and (b) for prolonged immersion (168–1200 h) in 0.1 M NaCl.
(a) |