Research Article

Protective Cerium-Based Layered Double Hydroxides Thin Films Developed on Anodized AA6082

Figure 12

SEM images after (a) 360 hrs of immersion, (b) 720 hrs of immersion, (c) 1200 hrs of immersion in 0.1 M NaCl solution.
(a)
(b)
(c)