Research Article
Experimental Investigation on Hydroabrasive Erosion of Steel Fiber UHPC and Rubber UHPC
Table 4
Steel fiber UHPC mix proportion (kg/m3).
| Group number | W/B | Steel fiber (%) | Type of aggregate | Slag powder (%) | Quartz powder (%) | Water reducing agent |
| A1 | 0.18 | 0.5 | NS | 17 | 8 | 7.5 | A2 | 0.18 | 1.0 | QS | 17 | 8 | 9 | A3 | 0.18 | 1.5 | SS | 17 | 8 | 8.5 | A4 | 0.20 | 0.5 | QS | 17 | 8 | 9 | A5 | 0.20 | 1.0 | SS | 17 | 8 | 11 | A6 | 0.20 | 1.5 | NS | 17 | 8 | 10.5 | A7 | 0.22 | 0.5 | SS | 17 | 8 | 10.5 | A8 | 0.22 | 1.0 | NS | 17 | 8 | 11.5 | A9 | 0.22 | 1.5 | QS | 17 | 8 | 13 |
|
|