Research Article

Influence of Tire-Recycled Steel Fibers on Strength and Flexural Behavior of Reinforced Concrete

Table 7

Flexural toughness index and residual strength coefficient of steel fiber reinforced concrete.

TypeNo.Flexural toughness indexResidual strength coefficient
I5I10I20I30R5,10R10,20R10,30

Industrial steel fibersI-52.383.215.148.4616.619.326.3
I-102.813.997.5514.7723.635.653.9
I-153.444.069.8715.8212.458.158.8
I-204.566.4810.8019.1538.443.263.4
I-255.489.9614.5926.4589.646.382.5

Tire-recycled steel fibersT-122.553.575.337.1620.417.618.0
T-183.145.337.1410.0543.818.123.6
T-243.876.039.8714.7143.238.443.4
T-304.266.0910.6918.7436.646.063.3
T-364.758.5714.8823.7576.463.175.9