Research Article
Shear-Dependent Yield Stress of Iron Ore Fine Tailings in Two-Step Flocculation Process
Table 1
Parameter design of floc shear disruption.
| | Primary broken phase | Secondary broken phase | | Shear rate | Shear time | Shear rate | Shear time |
| | 200 | 30 | 200 | 30 | | 400 | 30 | 400 | 30 | | 600 | 30 | 600 | 30 | | 800 | 30 | 800 | 30 | | 200 | 60 | 200 | 60 | | 400 | 60 | 400 | 60 | | 600 | 60 | 600 | 60 | | 800 | 60 | 800 | 60 | | 200 | 120 | 200 | 120 | | 400 | 120 | 400 | 120 | | 600 | 120 | 600 | 120 | | 800 | 120 | 800 | 120 | | 200 | 240 | 200 | 240 | | 400 | 240 | 400 | 240 | | 600 | 240 | 600 | 240 | | 800 | 240 | 800 | 240 |
|
|