Research Article
Compression Performance of Newly Designed Replaceable Tubular Steel Piers
Table 1
The design parameters of axially compressed specimens.
| Specimen label | f (MPa) | DS (mm) | H (mm) | D (mm) | t (mm) | t f (mm) | h (mm) |
| I-0 | — | — | 500 | 426 | 8 | — | — | I-A | — | 176 | 500 | 426 | 8 | — | — | II-A-1 | 160 | 67 | 500 | 426 | 8 | 10 | 410 | II-A-2 | 160 | 67 | 500 | 426 | 8 | 10 | 410 | II-A-3 | 160 | 67 | 500 | 426 | 8 | 10 | 410 | III-A-1 | 100 | 67 | 500 | 426 | 8 | 10 | 410 | III-A-2 | 160 | 67 | 500 | 426 | 8 | 10 | 410 | III-B-1 | 100 | 90 | 500 | 426 | 8 | 10 | 410 | III-B-2 | 160 | 90 | 500 | 426 | 8 | 10 | 410 | III-C-1 | 100 | 90 | 500 | 426 | 8 | 10 | 410 | III-C-2 | 160 | 90 | 500 | 426 | 8 | 10 | 410 | IV-A-1 | 160 | 67 | 500 | 426 | 8 | 10 | 410 | IV-A-2 | 160 | 67 | 500 | 426 | 8 | 10 | 350 | IV-A-3 | 160 | 67 | 500 | 426 | 8 | 10 | 290 |
|
|