Research Article
Compression Performance of Newly Designed Replaceable Tubular Steel Piers
Table 3
Summary results of axially compressed specimens.
| Specimen label | Nominal yield point | Peak point | Extreme point | Py/Pmax | Ductility | δy (mm) | Py (kN) | δmax (mm) | Pmax (kN) | δu (mm) | ax | μ = δu/δy |
| I-0 | 2.02 | 3250 | 5.69 | 3451 | 11.40 | 0.94 | 5.6 | I-A | 2.53 | 3250 | 6.68 | 3670 | 11.08 | 0.89 | 4.4 | II-A-1 | 1.84 | 2920 | 6.16 | 3284 | 10.74 | 0.89 | 5.8 | II-A-2 | 2.16 | 3071 | 6.44 | 3463 | 12.42 | 0.89 | 5.8 | II-A-3 | 1.89 | 2988 | 5.54 | 3359 | 11.31 | 0.89 | 6.0 | III-A-1 | 2.39 | 3433 | 5.35 | 3840 | 10.84 | 0.89 | 4.5 | III-A-2 | 2.02 | 3340 | 4.11 | 3760 | 8.24 | 0.89 | 4.1 | III-B-1 | 2.50 | 2927 | 7.24 | 3251 | 14.26 | 0.90 | 5.7 | III-B-2 | 3.38 | 2968 | 7.91 | 3302 | 14.97 | 0.90 | 4.4 | III-C-1 | 2.63 | 2977 | 8.55 | 3274 | 16.0 | 0.91 | 6.1 | III-C-2 | 1.75 | 2977 | 7.28 | 3199 | 20.07 | 0.93 | 11.5 | IV-A-1 | 2.37 | 3697 | 4.73 | 4137 | 12.85 | 0.89 | 5.4 | IV-A-2 | 2.21 | 3363 | 5.49 | 3849 | 12.81 | 0.87 | 5.8 | IV-A-3 | 2.02 | 3340 | 7.07 | 3707 | 22.80 | 0.90 | 11.3 |
|
|