Research Article
Damage and Degradation of Concrete under Coupling Action of Freeze-Thaw Cycle and Sulfate Attack
Table 3
Mix proportions in kg/m3 (except w/c) of concretes investigated in this study.
| | Cement | Fly ash | Coarse aggregates | Fine aggregates | Water w/c = 0.4 | Superplasticizer (%) | | % | kg |
| | 362.5 | — | — | 1211.2 | 681.3 | 145 | 1 | | 326.25 | 10 | 36.25 | 1211.2 | 681.3 | 145 | 0.7 | | 290 | 20 | 72.5 | 1211.2 | 681.3 | 145 | 0.5 |
|
|