Rheological Properties Comparing Hot and Cold Bituminous Mastics Containing Jet Grouting Waste
Figure 12
Accumulated strain results at the end of every 10 creep-recovery cycles of hot and cold bituminous mastics: (a) LH vs LC28d (I at 40°C and II at 60°C), (b) JH vs JC28d (I at 40°C and II at 60°C), and (c) LJH vs LJC28d (I at 40°C and II at 60°C).