Rheological Properties Comparing Hot and Cold Bituminous Mastics Containing Jet Grouting Waste
Table 3
Amount of mastic mixing materials per 100 gr of the study sample.
| Type | Filler-to-bitumen ratio (%) | Label | Materials (gr) | LF | JW | Water f/W = 0.5 (added + contained in BE) | B50/70 | BE (60% bitumen + 40% water) |
| Hot mastics | 0.3 | LH0.3 | 30 | — | — | 70 | — | JH0.3 | — | 30 | — | 70 | — | LJH0.3 | 15 | 15 | — | 70 | — | 0.4 | LH0.4 | 40 | — | — | 60 | — | JH0.4 | — | 40 | — | 60 | — | LJH0.4 | 20 | 20 | — | 60 | — | 0.5 | LH0.5 | 50 | — | — | 50 | — | JH0.5 | — | 50 | — | 50 | — | LJH0.5 | 25 | 25 | — | 50 | — |
| Cold mastics | 0.3 | LC0.3 | 30 | — | 60 (13.2 added + 46.8 contained in BE) | — | 117 (70.2 bitumen + 46.8 water) | JC0.3 | — | 30 | 60 (13.2 added + 46.8 contained in BE) | — | 117 (70.2 bitumen + 46.8 water) | LJC0.3 | 15 | 15 | 60 (13.2 added + 46.8 contained in BE) | — | 117 (70.2 bitumen + 46.8 water) | 0.4 | LC0.4 | 40 | — | 80 (40 added + 40 contained in BE) | — | 100 (60 bitumen + 40 water) | JC0.4 | — | 40 | 80 (40 added + 40 contained in BE) | — | 100 (60 bitumen + 40 water) | LJC0.4 | 20 | 20 | 80 (40 added + 40 contained in BE) | — | 100 (60 bitumen + 40 water) | 0.5 | LC0.5 | 50 | | 100 (66.8 added + 33.2 contained in BE) | — | 83 (49.8 bitumen + 33.2 water) | JC0.5 | | 50 | 100 (66.8 added + 33.2 contained in BE) | — | 83 (49.8 bitumen + 33.2 water) | LJC0.5 | 25 | 25 | 100 (66.8 added + 33.2 contained in BE) | — | 83 (49.8 bitumen + 33.2 water) |
|
|