Research Article
Mechanism of Secondary Deformation of Extruded AZ31 Magnesium Alloy by Viscoplastic Self-Consistent Model
Table 1
Hardening parameters of slip and twin systems in the simulation of Mg alloy under monotonic loading.
| Deformation mode | (MPa) | (MPa) | (MPa) | (MPa) | | | |