Research Article

Experimental Study on the Evolution Law of Mesofissure in Full Tailing Cemented Backfill

Table 4

Pore characteristic parameters of backfill.

In the loading stageCharacteristic parameter
Face rate (%)Fracture density (mm/mm2)Average pore size (μm)

Original specimen8.772.3221.37
Compaction stage7.281.6222.05
Elastic deformation stage9.243.2234.53
Plastic deformation stage17.116.5442.54
Postpeak failure stage25.4414.66266.41