Research Article
High-Temperature Tensile Fractography of Zr-, Ni-, and Mn-Containing Al-Si-Cu-Mg Cast Alloys
Figure 12
Cross sections beneath the fracture surface of M1S alloy: (a) T6 condition and (b) after stabilization at 250 C for 200 h. The blue arrow indicates the tensile testing direction.
(a) |