Research Article
Influence of Antistripping Additives and Rejuvenators on Healing Performance of Moisture-Damaged HMA
Table 3
Mix proportion of aged series.
| | ā | Aged binder (by wt. of total mix) | Additive agent (by wt. of binder) | SWF (by wt. of binder) | | PAV5 | PAV15 | PAV20 | C | Type 2 | Type A |
| | Induction heating | 5.4% | 2% | 6% | | Microwave heating | 5.4% | 2% | 2% |
|
|